Abstract

Pulverized Coal Injection (PCI) is a key technology in modern ironmaking by blast furnace and the life of injection lance has a great influence on PCI operation and on normal running of blast furnace. It is found that the main reasons for the failure of the lances are their outer surface oxidation and the inner surface erosion through monitoring some lances used in BF. The outer surface oxidation of the lances made of lCr18Ni9Ti is inevitable under high hot blast temperature condition through thermodynamics analysis. Increasing the inner surface hardness by surface treatment would prolong the service life of coal lance. The anti-oxidation temperature of lance materials needs to be over 1000°C for BF intensified smelting.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.