Cyclic oxidation of Fe-20Cr-4Al alloys with small amounts of sulfur contained was studied up to 5 cycles (1 cycle=18.0ks) at 1473K in oxygen. Adherence of oxide scales on Fe-20Cr-4Al-(3, 104 and 171ppm) S alloys was improved by sulfur. On the other hand, oxide scales on Fe-20Cr-4Al-(35 and 53ppm) S alloys spalled markedly after 1-3 cycles, and amounts of spalled oxide of the alloys decreased after 4-5 cycles.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.