Abstract
The curing reaction of epoxy resin Epidian® 6 with or without an addition of reactive filler, octakis-[(3-glycidoxypropyl)dimethylsiloxy]octasilsesquioxane (POSS-OG), was investigated using differential scanning calorimetry (DSC). The curing agent was 4,4'-diaminodiphenylmethane (DDM). Based on the analysis of the thermograms recorded at different heating rates the kinetics of curing reactions in the examined systems was determined using the Model Free Kinetics method. The experimental results obtained by DSC isothermal analysis in the temperature range 60—160 °C, with temperature modulation TOPEM®, were used to construct TTT (time-temperature-transformation) diagram for epoxy resin Epidian 6 compositions with or without POSS-OG.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.