In this letter we report on CulnSSe-doped glasses used as a saturable absorber for passive mode-locking of a Nd:YAG and Nd:YAlO3 lasers. Ultrashort pulses of 16 ps duration with 20 µj of energy (for YAlO3 at 1.08µm), and 36 ps duration with 45µj of energy (for YAG at 1.064µm) are achieved, respectively. The bleaching relaxation time of CuInSSe-doped glass saturable absorber is found to be ~11 ps. The optical damage threshold for CuInSSe-doped glasses estimated from the intensity dependent transmittance measurement with the use of laser pulses of 15 ps duration was ~20 GW/cm2.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.