Abstract

The PLZT (3/66/34), PLZT (3/46/54), PLZT (9/65/35) and PLZT (28/0/100) thin films were deposited on MgO (100), Sapphire (0001) and fused silica substrates by using pulsed KrF excimer laser deposition technique. The conventional in-situ and 2-step heating processes were utilized to facilitate the synthesis of a large area of uniform PLZT thin film. Pure perovskite phase can be obtained only under very narrow process conditions, the highly textured PLZT films can be easily obtained by in-situ heating process. For PLZT (28/0/100) material, epitaxial films were successfully coated on MgO (100) substrates by 600°C in-situ and RTA 650°C 2-step heating processes. The latter was found to possess higher refractive index and lower extinction coefficient.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.