Abstract
2D dislocation dynamics simulations were used to investigate the size effect observed experimentally in the yield behavior of micrometer-sized crystals of γ–γ′ superalloys. Random Frank–Read sources were introduced on a (1 1 1) glide plane for three simulation cell sizes. Critical stresses were determined for the percolation of dislocations evolving from the Frank–Read sources in such cells populated with a distribution of γ′ precipitates at ∼73.5% by volume, consistent with the experiment. An APB energy of 250 mJ m−2 was used in the simulations. The study found that the simulation results of percolation stresses were consistent with experimental 0.2% yield stress values with respect to both the scatter at each sample size, as well as the weak variation in critical stress with size. The weak size effect and the large scatter were found to be related to two factors: () strength of single-arm sources, as well as () the variation in precipitate structure at the single-arm source positions.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
More From: Modelling and Simulation in Materials Science and Engineering
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.