Abstract
Alloy 22 is a nickel base alloy highly resistant to all forms of corrosion. It was designed to resist to most aggressive environments for industrial applications. Electrochemical studies such as Potentiodynamic-Galvanostatic-Potentiostatic (PD-GS-PD) tests and Electrochemical Impedance Spectroscopy (EIS) and Scanning Electron Microscopy (SEM) observations were performed to determine the corrosion behaviour of alloy 22 (N06022). The effect of sulphate ion in chloride containing solutions at 90°C, were studied in this work under aggressive conditions where this material might be susceptible to crevice corrosion. The electrolyte solution, which consisted of 0.1M and 1M NaCl and different sulphate concentrations. It was observed that there were complete inhibitions of crevice corrosion for Rcrit=[SO4=]/[Cl-]=1 in the 0.1mol/L NaCl solutions and Rcrit=2 in the 1mol/L NaCl solutions. The corrosion rate obtained was about 0.1μm/year at 24 hours of immersion.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.