This work studies the creep rupture behaviors of both smoothed and V-notched DD6 Ni-based single crystal superalloy specimens under both air and corrosion conditions, within a stress range of 300 to 700 MPa at 950 °C. The corrosive medium used consisted of a mixed salt containing 95 wt% Na2SO4 and 5 wt% NaCl. Experimental results revealed that notched specimens exhibited a creep rupture life extended by 6–16 times compared to smoothed specimens, with the extension becoming more pronounced as the stress concentration increased. High-temperature hot corrosion (HTHC) shortened the creep rupture time by up to 75 %. A significant HTHC-creep interactive effect was found through comparative creep experiments in air and corrosion conditions. The HTHC affected the fracture modes of the specimens, with factors such as the amount of salt infiltration into the superalloy, the corrosion duration, and specimen configurations playing critical roles. Microstructural analysis revealed that, compared with γ′ precipitates, γ matrix phase was more prone to creep damage and was more susceptible to corrosion.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.