Process for getting crack-free lead zirconate titanate (PZT) thin films micropatterned on Si substrate is demonstrated. The PZT film was deposited at temperatures below 300°C by magnetron sputtering using a ceramic target, and then etched before annealing. After annealed above 500°C to get perovskite phase, the PZT films shows no crack, while PZT films, not patterned, has cracks. This result can be explained as dissipation of stress energy by reduction of the lateral size of the film. The effects of processing parameters of reactive sputtering and annealing on the morphology of the PZT thin films are presented. Photo-assist etching of the PZT thin films using KrF laser is described, too.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.