In the laser machining of ceramics, it is difficult to avoid the formation of a recast layers and cracks. These deffects significantly spoil some excellent properties of ceramics. This paper describes the feasibility of a crack-free processing method. for hot-pressed silicon nitride (Si3N4) ceramics with an yttrium aluminum garnet (YAG) laser. It is found that, in order to attain the defect-free machining, it is necessary to process the ceramics using a laser beam pulsed below 500 ns in duration and 10 kHz in repetition rate.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.