A variety of commercially available ceramic‐based oxides, carbides, nitrides, and borides were evaluated for chemical attack in an azeotropic aqueous hydrofluoric acid (HF) test protocol at 90°C. Weight change measurements and microstructure analysis showed that HF corrosion in polycrystalline ceramics generally occurred at grain boundaries by the dissolution of grain boundary phases although the bulk single crystal may inherently resist attack. Virtually all commercially prepared polycrystalline oxide ceramics (i.e., Al2O3, TiO2, ZrO2) and nonoxide ceramics (i.e., Si3N4, AlN, BN) were extensively corroded while polycrystalline pure carbides (i.e., SiC, TiC, B4C, WC) resisted corrosion. Equilibrium thermodynamic calculations show that these materials are soluble in HF; however, the kinetics of dissolution are slow enough in some cases to permit useful engineering lifetimes.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.