The present work discusses corrosion behavior of newly developed bainitic steels made by isothermal heat treatment of a new steel composition (0.71 pct C, 1.15 pct Mn, 0.20 pct Ni, 0.59 pct Cr, 0.40 pct Cu, 0.35 pct Si, 0.026 pct S, 0.027 pct P, and rest Fe (weight percent)). Corrosion behavior of the pearlitic steel made by normalization is also studied. Electrochemical polarization and salt fog tests are carried out in 0.6 M NaCl. Steel rusts after salt fog tests are analyzed. Modified composition, finer microstructures, and compact rust morphology attribute to better corrosion resistance of the bainitic steels. Corrosion mechanisms for the pearlitic and bainitic steels are discussed.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.