Abstract
The paper studies structure and phase characteristics of the interphase zone diamond/matrix in dressers made by thermal diffusion metallization of a diamond combined with matrix sintering based on WC–Co and Cu impregnation. The compact arrangement of chromium powder particles around diamond grains and the shielding effect of copper foil create favorable conditions for thermal diffusion metallization of diamond at matrix sintering. A metallized coating chemically bonded with diamond and consisting of chromium carbide and solid solution of cobalt in chromium phases provides a strong diamond retention in the carbide matrix. It was shown that it is formed on the surface of the diamond under the conditions specified in the experiment and the temperature – time sintering mode. The specific productivity of experimental dresser made by hybrid technology at straightening green silicon carbide grinding wheel equaled 51.50 cm3/mg exceeding that of the control dresser made without metallization of diamonds by sintering with copper impregnation by 44.66%.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.