Abstract

It is extremely desirable but challenging to develop exchange-coupled magnets with well-dispersed hard/soft phase and confined size to meet the high energy requirements of advanced magnets in modern industry and information technology. Here, we report a novel bottom-up strategy with two-step thermal decomposition and reductive annealing process to synthesize Nd₂Fe₁₄B/α-Fe nanocomposites, in which effective control of the hard/soft magnetic phase size and proportion was achieved. It is worth noting that the composition, as well as phase distribution, can be readily tuned by changing the ratio between Nd-Fe-B-oxide and α-Fe. This work provides an effective approach to adjust the phase size and distribution for exchange-coupled, rare-earth nanomagnets, which can be fundamental for high energy magnets.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.