Abstract

We present a study on the electrochemical behavior of magnesium hydroxide (MgOH+) reduction on a tungsten (W) cathode in molten chloride salt (MgCl2-KCl-NaCl) across the temperature range of 475 °C–525 °C. MgOH+, which forms within the salt upon exposure to moisture, is a leading cause of corrosion. Corrosion is a major barrier to deployment of chloride salts across a number of applications, including concentrating solar power plants and nuclear power plants. While pre-purification protocols have been developed to ensure MgOH+ is removed from molten chloride salts prior to deployment, MgOH+ forms in situ during operation of chloride-salt based plants. Thus, methods for continuous purification during plant operation are needed. Continuous electrochemical purification via electrolysis using a Mg anode and W cathode has been proposed, but little has been done to assess scalability. Here, we assess fundamental properties of electrochemical removal of MgOH+ to enable future scale up of this method.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.