Abstract

This research aims to construct hydrotalcite Mg-Al-CO3 by tuning the pH synthesis and molar ratio. The tuning was carried out by applying different synthesis pH. In addition, utilization of snail shell waste is expected to replace CO3 2- ion that needed for anion component in hydrotalcite production. For this study precipitation and hydrothermal methods were applied for synthesis. The precipitation had been carried out in three steps, namely isolation of ion CO3 2- from snail shell, preparation of Na2CO3 solution using snail shell powder as ion CO3 2- source and synthesizing hydrotalcite, where hydrothermal method was carried out at 150 °C. Confirmation of hydrotalcite obtained was done using SEM and FTIR.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.