Abstract

He-ion irradiation simulating α-particle emission, induces crystal defect recovery in fluoroapatite Ca 10(PO 4) 6F 2 pre-damaged by Pb-ions. In fluoroapatite loaded with α-emitter actinides, a similar effect is expected. Therefore, the amorphization level in fluoroapatite has been modeled versus disposal time, α-decay fluence and temperature. When loaded with 239 Pu and 244 Cm , the structural disorder reaches a plateau, which level depends only slightly on α-energies. This level corresponds to an amorphous fraction of approximately 20% of disorder and is independent of the dose rate. The time delay in reaching the equilibrium regime in the disorder production is inversely proportional to the dose rate whereas the dose or the actinide content is not a critical parameter for the magnitude of the equilibrium level.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.