The interfacial compatibility of an alkaline earth silicate glass (SABS-0) with (Mn,Co) 3O 4 coated Crofer 22 APU and AISI 441 interconnects has been investigated at 800 °C for 100 h in argon, air, and H 2/H 2O atmospheres. Detailed microstructural and diffusion studies show that the interfacial compatibility is better for the (Mn,Co) 3O 4 coated Crofer 22 APU alloy but deteriorates from the H 2/H 2O to the air or the argon atmospheres for both alloys. Thermal treatment atmosphere mainly affects the inter-diffusion of Cr in the Crofer 22 APU alloy. The (Mn,Co) 3O 4 layer cannot eliminate the undesirable Cr diffusion for the Crofer 22 APU alloy regardless of the thermal treatment atmosphere. The interfacial reaction for the AISI 441/SABS-0 is so severe that the inter-diffusion of the elements is less significant. Oxidation of the AISI 441 alloy degrades the (Mn,Co) 3O 4 coating stability and increases the reaction of the coating with the SABS-0 glass, leading to inferior interfacial compatibility.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call