Abstract

The purpose of this study was to compare the osteogenic potential of a synthetic and a demineralized bone matrix (DBM) putty using a cranial defect model in New Zealand white rabbits. Paired, bilateral critical-size defects (10 mm) were prepared in the frontal bones of 12 rabbits and filled with either OsteoSelect DBM Putty or NovaBone calcium-phosphosilicate putty. At days 43 and 91, 6 rabbits were killed and examined via semiquantitative histology and quantitative histomorphometry. Defects filled with the DBM putty were histologically associated with less inflammation and fibrous tissue in the defect and more new bone than the synthetic counterpart at both time points. Histomorphometric analysis revealed that the defects filled with DBM putty were associated with significantly more bone formation at day 43 (70.7% vs 40.7%, P = 0.043) and at day 91 (70.4% vs 39.9%, P = 0.0044). The amount of residual implant was similar for both test groups at each time point.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.