Abstract

The morphology of alkali–silica gel formed in dolomitic limestone affected by the so-called alkali–carbonate reaction (ACR) is compared to that formed in a siliceous limestone affected by alkali–silica reaction (ASR). The particle of dolomitic limestone was extracted from the experimental sidewalk in Kingston, Ontario, Canada that was badly cracked due to ACR. The siliceous limestone particle was extracted from a core taken from a highway structure in Quebec, affected by ASR. Both cores exhibited marked reaction rims around limestone particles. The aggregate particles were polished and given a light gold coating in preparation for examination in a scanning electron microscope. The gel in the ACR aggregate formed stringers between the calcite crystals in the matrix of the rock, whereas gel in ASR concrete formed a thick layer on top of the calcite crystals, that are of the same size as in the ACR aggregate.

Full Text
Published version (Free)

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call