Abstract
The measurement of the film thickness of the composite cement Variolink Esthetic («Ivoclar-Vivadent», Liechtenstein) and the microhybrid composite Enamel («Micerium», Italy) was carried out according to ISO 4049: 2009 standards with a load force of 5 kg. While reducing the load force to 5 kg, all materials showed an increase in the film thickness; the film thickness of the Variolink Esthetic composite cement was changed from 23 microns (at 15 kg) to 32 microns (at 5 kg), and the film thickness of the microhybrid composite film Enamel was changed from 39 microns (at 15 kg) to 102 microns (at 5 kg). After preheating, the film thickness was changed from 23 microns (at 15 kg) to 44 microns (at 5 kg).
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.