Abstract
PurposeThis paper aims to understand the effect of water jet cavitation peening (WJP) on stress corrosion cracking (SCC) behavior of alloy 600 and alloy 182 in high temperature water.Design/methodology/approachSurface and cross-section morphology, grain boundary microstructure, residual stress and strain distribution, hardness and surface roughness in water jet cavitation peened alloy 600 and alloy 182 were characterized.FindingsA superior stress corrosion cracking resistance was obtained in 600MA, which can be attributed to the formation of the ultrafine grain layer and the higher magnitude residual compressive stress.Originality/valueRelationship between WJP-induced microstructure and stress state change and SCC susceptibility was conducted. It could provide a theoretical basis for developing application of WJP in nuclear power plants.