Abstract

Abstract Blends of uncrosslinked styrene-butadiene rubber (SBR) with a terpene tackifier resin or a naphthenic oil have been characterized, and their autohesion and cohesion determined using a T-peel geometry. SBR/oil blends are homogeneous at all proportions, while SBR/resin blends, based on DSC and DMA analysis, undergo bulk phase separation at about 50% resin. However, migration of tackifier to the surface region is proposed at much lower resin contents. Compositions diluted with oil have autohesion similar to the neat SBR. This is attributed to compensating effects; although oil hastens self-bond formation by increasing chain mobility, this is nearly equally balanced by more facile chain separation during bond rupture. In short, oil-diluted compositions are soft and weak. On the other hand, SBR compositions containing small amounts of resin have high autohesion. Resin-diluted specimens deform easily at low strain, just as those containing oil, but intertwined chains of the former have greater resistan...

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.