Abstract

AbstractThe Fourier transformed infrared (FTIR) spectroscopy on the rubber‐filler gel has been used as a tool for the quantitative characterization of the phase selective silica localization in styrene butadiene rubber (SBR)/natural rubber (NR) blends. The so‐called rubber‐layer L was introduced to describe the selective wetting behavior of the rubber phases to the filler. SBR/NR blends filled with silica were the focus of the experimental investigation. NR shows a higher wetting rate than SBR. Silane addition does not affect the wetting of NR but slowdowns the wetting of SBR. With increasing chamber temperature the value of the rubber‐layer L of all mixtures increases owing to the different thermal activated rubber‐filler bonding processes. Using the wetting concept the kinetics of silica localization in the phases of heterogeneous rubber blends was characterized. Because of the higher wetting rate of the NR component, in the first stage of mixing of NR/SBR blends more silica is found in the NR phase than in the SBR phase. In the next stage, silica is transferred from the NR phase to the SBR phase until the loosely bonded components of NR rubber‐layer are fully replaced by SBR molecules. POLYM. COMPOS., 31:1701–1711, 2010. © 2010 Society of Plastics Engineers.

Full Text
Published version (Free)

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call