A comprehensive study was carried out on four different fly ashes used as a catalyst for the degradation of Acid Red 1 using ultraviolet rays. These fly ashes are collected from different thermal power stations located at various places in India and having different chemical compositions. Three fly ashes are from lignite-based thermal power plants, and one is from the coal-based power plant. One fly ash is classified as Class F, two fly ashes are classified as Class C and remaining one is not conforming to ASTM C618 classification. X-Ray Fluorescence analysis was used to identify the chemical composition of fly ashes and SiO2, Al2O3, CaO, Fe2O3 and TiO2 were found to be the major elements present in different proportions. Various analysis were carried out on all the fly ashes like Scanning Electron Microscopy to identify the microphysical properties, Energy Dispersive X-Ray spectroscopy to quantify the elements present in the catalyst and X-Ray Diffraction to identify the catalyst phase analysis. The radical generated during the reaction was identified by Electron paramagnetic resonance spectroscopy. The parameters such as initial pH of the dye solution, catalyst dosage and initial dye concentration which influence the dye degradation efficiency were studied and optimised. In 60 min duration, the dye degradation efficiency at optimum parametric values of pH 2.5, initial dye concentration of 10 mg/L and catalyst dosage of 1.0 g/L using various fly ashes, i.e., Salam Power Plant, Barmer Lignite Power Plant, Kutch Lignite Power Plant and Neyveli Lignite Thermal Power plant (NLTP) were found to be 40, 60, 67 and 95 % respectively. The contribution of adsorption alone was 18 % at the above mentioned optimum parametric values. Among the above four fly ash NLTP fly ashes proved to be most efficient.
Published Version
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have