Abstract
Report is given on the combustion and pyrolysis conditions. The analytical procedure is described. During combustion and pyrolysis of pure polyvinylchloride (PVC) and PVC-cable sheathings in an air atmosphere, PCDD/PCDF are formed in significant amounts up to the ppm range. In general furans were formed predominantly. Especially higher levels of octa- and heptachlorinated furans were generated in the pyrolysis experiments, whereas lower chlorinated furans were produced predominantly by combustion.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.