Abstract
The paper described the shock-wave synthesis of high-pressure high-temperature mineral MgAl2O4 with the parameter a = 8.085(3) A and the Laves phase MgCu2 with a = 7.076(2) A from a mixture of MgO and aluminum powder placed into a copper insert inside a steel conservation ampoule. Spinel MgAl2O4 with a smaller lattice parameter a = 8.0798 A has been formed in an aluminum insert cup.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.