(1) Background: The purpose of this in vitro study was to evaluate the color change and stability of a zinc oxide nanoparticle-poly(methyl methacrylate) (ZnO NP-PMMA) nanocomposite for denture base material after immersion in different dietary and cleaning agent solutions. (2) Methods: One hundred samples were prepared and divided into four equinumerous groups depending on the weight content of ZnO NPs. The color coordinates (CIE L*a*b*) were measured using a digital colorimeter, ColorReader (Datacolor AG Europe, Rotkreuz, Switzerland), before and after immersion of the specimens in five different solutions (distilled water, coffee, red wine, black tea, denture cleaning tablet solution) for 6 months. The color changes (ΔE) were calculated using Euclidean distance and analyzed by the Shapiro-Wilk test and the ANOVA/Kruskal-Wallis multiple comparison and adequate post hoc tests. (3) Results: All tested materials showed significant color changes after their exposure to all solutions. Color changes were greatest in the case of red wine and progressed with the duration of the study. (4) Conclusions: The modification of PMMA with ZnO nanoparticles is acceptable in aesthetic terms in 2.5% and 5% weight content; however, color changes are more noticeable with higher nanoparticle content and must be discussed with the patient prior to possible use.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.