Abstract

Pure and Co-doped ZnO nanoparticles were synthesized with different cobalt levels (1–10 mol%) via adapted sol–gel method using water as solvent and characterized by X-ray diffraction, transmission electron microscopy, Raman spectroscopy and photoacoustic absorption spectroscopy. The results showed that all the samples have hexagonal wurtzite structure, with no evidence of any secondary phases until 10 mol% of the dopant. The average crystallite size of the samples was in the range of 25–50 nm, do not showing significant differences with the increase of the dopant level. However, the band gap energy of the nanoparticles decreases from 2.98 eV (pure ZnO) to 1.95 eV (10 mol% of Co). The photocatalytic activity of the samples was evaluated on the removal of methylene blue under visible light irradiation, which revealed an efficiency reduction by Co-doping ZnO. The antibacterial property was carried out indicating activity of the prepared samples against gram-positive bacteria.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.