The present work deals with synthesizing the pure ZnO (PZ), manganese-doped ZnO (MZ), and manganese-cobalt co-doped ZnO (MCZ) nanoparticles by hydrothermal method. X-ray diffraction confirms their hexagonal wurtzite structure with varying crystallite sizes: 43.8 nm for PZ, 34.6 nm for MZ, and 27.6 nm for MCZ. The band gap values were calculated as 3.14 eV (PZ), 3.09 eV (MZ), and 2.89 eV (MCZ) from Tauc plot. FTIR analysis provided the evidence of metal–oxygen bonds and other characteristic functionalities. These nanoparticles exhibited potent antibacterial activity against both gram-positive (Bacillus subtilis and Staphylococcus aureus) and gram-negative (Escherichia coli and Pseudomonas aeruginosa) bacteria. In photocatalytic performance of MCZ has showed a higher rate of Crystal Violet dye degradation under visible light irradiation compared to other materials.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.