Abstract

A SiC dry etcher using chlorine trifluoride (ClF3) gas was evaluated, particularly about the etching rate distribution. At 100%, the etching rate was high in the center region and was low in the outer region. However, that at 20% showed the opposite profile. This difference was considered to be due to the chlorine trifluoride gas distribution which was built above the gas distributor.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.