Abstract

Aligned chitosan nanofibers exhibiting diameters smaller than 100nm were easily prepared by combining ultrasonic atomization with freeze casting. A major advantage of this approach is the use of distilled water as main solvent. Scanning electron microscopy demonstrated that fiber diameter and morphology mainly depended on the atomizing tools, freezing temperature, and chitosan solution viscosity. Minimum diameter and uniform orientation were achieved using an electric flosser as an atomizing tool, liquid nitrogen as a coolant, 0.4wt% aqueous chitosan solution (molecular weight=22kDa), and a small amount of lactic acid as solvent at 0°C. The resulting chitosan nanofibers may find application in biomedical and food engineering. Moreover, this new technology may be applicable to other natural and synthetic water-soluble polymers.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.