Abstract

AbstractNi0.5Co0.2Mn0.3(OH)2 spherical precursor with an average particle size of 9.88 μm is prepared via co‐precipitation from an aqueous solution of NiSO4, CoSO4, and MnSO4 (Ni:Co:Mn = 5:2:3) using NaOH as precipitating and oxalic acid as chelating/reducing agent.