Abstract

AbstractThe title compounds are prepared by heating mixtures of Nd2O3 or Sm2O3, Al2O3, and graphite powder under N2 between 1000 and 1350 °C (alumina boat, about three 10 h cycles).

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.