Abstract

This study investigated the coagulation performance of titanium tetrachloride (TiCl4) for leachate treatment and preparation of titanium oxide (TiO2) from generated sludge through calcination process at different temperatures and times. TiCl4 with chitosan as coagulant aid employed to perform coagulation process on Alor Ponhsu Landfill leachate. Further calcination process was done to synthesize TiO2 from produced sludge for photocatalytic applications. The studied factors included pH, TiCl4 dosage, and chitosan dosage. The results indicated that maximum reduction in suspended solids was 92.02% at pH 4, 1200 mg/L TiCl4, and 250 mg/L chitosan addition, and maximum reduction in chemical oxygen demand was 71.92% at experimental condition of 1200 mg/L TiCl4 and 500 mg/L chitosan with pH 10. The maximum and minimum band gaps of prepared TiO2 achieved at 3.35 eV and 2.75 eV, respectively. Morphology and phase analysis of prepared TiO2 characterized using scanning electron microscope (SEM) and X-ray diffraction (XRD). The XRD spectrums showed theanatasephase at lower calcination temperature and therutilephase at elevated temperature. The photocatalysis activity of produced TiO2 investigated under UV irradiation and showed almost fast degradation similar to commercial TiO2. The results indicated that TiO2 powder was successfully prepared from generated sludge from TiCl4 coagulation for photocatalytic applications.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.