Process and material characterization of the crystallization of amorphous silicon by metal-induced crystallization (MIC) and metal-induced lateral crystallization (MILC) using evaporated Ni has been performed. An activation energy of about 2 eV has been obtained for the MILC rate. The Ni content in the MILC area is about 0.02 atomic %, significantly higher than the solid solubility limit of Ni in crystalline Si at the crystallization temperature of 500/spl deg/C. A prominent Ni peak has been detected at the MILC front using scanning secondary ion mass spectrometry. The MIC/MILC interface has been determined to be highly defective, comprising a continuous grain boundary with high Ni concentration. The effects of the relative locations of this interface and the metallurgical junctions on TFT performance have been studied.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.