Abstract

We present an experimental characterization of the amplification of sub-nanosecond duration laser pulses at a wavelength of 1538 nm in short custom-made Er:Yb phosphate glass fibers with different core diameters. The fibers vary in their diameter from 100 µm (highly multi-mode) down to 12 µm (single-mode). The peak power, energy per pulse, and spectral shape of the amplified signal are presented. With our input pulses, the measurements show that the large core diameter fibers do not increase the amplification of the 1538 nm signal. We believe this is due to the high re-absorption of the Er3+ ions in the phosphate fiber. The optimal fiber geometry was found to have a core diameter of 20 µm with a length of 14 cm. The maximum peak power is 8.25 kW, corresponding to a net gain of 10.9 dB, with a pulse duration of 0.7 ns and a repetition rate of 40 kHz.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.