Abstract
The thermal properties of semiflexible thermotropic polyesters and low molecular mass model compounds were investigated by differential scanning calorimetry. An account is given of some peculiar aspects strictly related to the polymeric nature of the specimens. In particular, the influence of molecular mass and thermal treatments on the transition temperatures of the polymers is evidenced. The occurrence of polymesomorphism was revealed by the appearance of multiple DSC peaks.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.