Abstract

Ultra-thin films of hafnium oxide deposited on Si(1 0 0) substrates by means of atomic layer deposition using tetrakis(diethylamino)hafnium as the hafnium precursor are characterized. These films and interface structures are probed using Fourier transform infrared spectroscopy along with Z-contrast imaging and electron energy loss spectroscopy (EELS) of a scanning transmission electron microscope. The interface structure of HfO 2/Si(1 0 0) is further investigated using angle resolved X-ray photoelectron spectroscopy to probe the core level orbitals (Hf 4f, Si 2p, O 1s) at high resolution. The interfacial differences are also examined by probing the Hf 4f bonding with normal incidence XPS in thin and thick films. The XPS studies show that the binding energies remain unchanged with film depth and that there is no apparent signature of silicate structure in the as-deposited films. EELS spectra taken at the interface and XPS measurements suggest the interface is mainly silicon oxide. Two different cleaning methods used show difference only in the thickness of the silicon oxide interlayer.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.