Abstract

Delamination failure criterion is an important tool for characterizing the fracture behavior of laminated composites under mixed loading. In this paper, a fracture envelope was built based on the energy release rate as a fracture criterion of graphite/PEEK laminates. Unidirectional cracked lap shear (CLS) specimens were employed to calculate mode I and mode II energy release rates ( G I, G II. Static fracture tests were conducted using the specimens with two different lap to strap thickness ratios in order to obtain a wide range of G I/ G II values. The G I/ G II values for each thickness ratio were calculated numerically using finite element analysis. The results showed that as a delamination length changes, the G I/ G II varies from 0.13 to 0.48 depending on the lap to strap thickness ratio. It was also found that a linear fracture envelope may be appropriate for a CLS composite specimen.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.