Abstract

The Cd[Formula: see text]Zn[Formula: see text]O thin films have been deposited on glass and Si substrates at room-temperature with different Cd contents (x = 0, 2%, 4% and 6 wt.%) by pulsed laser deposition (PLD) technique. X-ray diffraction (XRD) analyses evidenced that the films possess polycrystalline and a hexagonal ZnO crystal structure for x = 0, 2% and 4% with a preferred orientation in the a-axis (101) direction, while films with a mixed hexagonal and cubic structure was revealed for x = 6 wt.%. Electrical measurement presented that the resistivity decreased with increased temperature and concentration of Cd. The deliberated activation energy was reduced was from 0.224 to 0.113 eV with increase doping concentration. Current–voltage (I–V) and capacitance–voltage (C–V) characteristics of the fabricated Cd[Formula: see text]Zn[Formula: see text]O/p-Si heterojunction varied with the applied bias and the Cd concentration. The results of the values of built-in potential (V[Formula: see text]) and the ideality factor (n) increased with raising Cd concentration.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.