Abstract

Blends of high density polyethylene (HDPE) and polypropylene (PP) with different biodegradable additives have been subjected to an outdoor soil burial test. The effect of the degradation process on the structural and morphological properties of the samples has been studied by thermogravimetry, differential scanning calorimetry, and dynamic-mechanical spectroscopy. The thermogravimetric results show that the additive is more affected by the degradation process than the polymeric matrix. Changes both in the crystalline morphology and the activation energies of the relaxation processes take place in different stages, and can be described using polynomial equations. These changes occur on different time scales depending on the additive used. © 2002 Wiley Periodicals, Inc. J Appl Polym Sci 86: 174–185, 2002

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.