Natural bearing (raw and calcined at 500 °C) and iron-enriched (impregnation and pillaring) montmorillonitic clay samples were prepared. The obtained samples were characterized (X-ray diffraction, Fourier Transformed Infrared Spectroscopy, Scanning Electron Microscopy, and Energy Dispersive X-ray Spectroscopy) and evaluated as catalysts in catalytic wet oxidation of Brilliant Green and Crystal Violet. Experiments were conducted in the same conditions (0.5 g catalysts, 300 mL air/min or 0.5 mL H2O2, 25 mL of dye solution, 25 °C, initial solution pH = 6.0, for 3 h) in thermostated batch reaction tubes. Process evolution was followed using UV-Vis spectrometry (200–1100 cm−1) and total organic carbon. Dye removal efficiencies (decolorization) between 98 and 99% were determined, while total organic carbon removal efficiencies were calculated to be in the 53–98% range. Iron leakage investigation showed that iron is lost in higher amounts for the catalysts prepared using the impregnation method by comparison with the pillared sample.

Full Text
Published version (Free)

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call