Abstract

Cd x Zn 1− x Se films (0 ⩽ x ⩽ 1) were deposited for the first time by the pulse plating technique at different duty cycles in the range 6–50% at room temperature from an aqueous bath containing zinc sulphate, cadmium sulphate and selenium oxide. To the author’s knowledge this is the first report on pulse plated Cd x Zn 1− x Se films. The deposition potential was −0.9 V (SCE). The as deposited films exhibited cubic structure. Composition of the films was estimated by Energy Dispersive Analysis of X-ray studies. X-ray photoelectron spectroscopy studies indicated the binding energies corresponding to Zn(2p 3/2), Cd(3d 5/2 and 3d 3/2) and Se(3d 5/2 and 3d 3/2). Optical band gap of the films varied from 1.72 to 2.70 eV as the composition varied from CdSe to ZnSe side. Atomic force microscopy studies indicated grain size in the range of 20–150 nm.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.