ABSTRACTDeep borehole disposal (or DBD) is now seen as a viable alternative to the (comparatively shallow) geologically repository concept for disposal of high level waste and spent nuclear fuel. Based on existing oil and geothermal well technologies, we report details of investigations into cementitious grouts as sealing/support matrices (SSMs) for waste disposal scenarios in the DBD process where temperatures at the waste package surface do not exceed ∼190ºC. Grouts based on Class G oil well cements, partially replaced with silica flour, are being developed, and the use of retarding admixtures is being investigated experimentally. Sodium gluconate appears to provide sufficient retardation and setting characteristics to be considered for this application and also provides an increase in grout fluidity. The quantity of sodium gluconate required in the grout to ensure fluidity for 4 hours at 90, 120 and 140°C is 0.05, 0.25 and 0.25 % by weight of cement respectively. A phosphonate admixture only appears to provide desirable retardation properties at 90°C. The presence of either retarder does not affect the composition of the hardened cement paste over 14 days curing and the phases formed are durable under conditions of high temperature and pressure.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.