Abstract

ABSTRACT Due to increased copper production and the associated environmental consequences, copper production processes need to be improved, considering the impact of their byproducts, among others slag. This study investigated the leaching of individual constituents of iron silicate slag from a copper smelter. This was done by characterising granulated samples of its constituents – glass, matte, speiss – to determine their leaching contribution. It was observed that leaching in distilled and deionised water without pH regulation achieved various natural pH for the constituents. At natural pH, glass (Cu, Zn) and speiss (Ni, Sb) contributed to leaching. Static pH titrations showed the increased leaching of Zn, Cu, Ni, As, and Sb with decreasing pH. The results showed that, an iron silicate slag consisting of glass, matte and speiss, contributes to leaching as follows: matte – Cu and Ni, speiss – Cu, Ni, As, and Sb. Zn leaching is similar among the constituents.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.