Abstract

We demonstrated the successful growth of catalyst-free InN nanorods on (0001) Al2O3 substrates using metal-organic chemical vapor deposition. Morphological evolution was significantly affected by growth temperature. At 710 degrees C, complete InN nanorods with typical diameters of 150 nm and length of approximately 3.5 microm were grown with hexagonal facets. theta-2theta X-ray diffraction measurement shows that (0002) InN nanorods grown on (0001) Al2O3 substrates were vertically aligned along c-axis. In addition, high resolution transmission electron microscopy indicates the spacing of the (0001) lattice planes is 0.28 nm, which is very close to that of bulk InN. The electron diffraction patterns also revealed that the InN nanorods are single crystalline with a growth direction along (0001) with (10-10) facets.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.