1. To obtain a high case hardness it is necessary to reach, during carburizing, a saturation degree in excess of 2% C. Carburizing must be conducted at 950 or 100° C for 15 or 5 hrs. to obtain a total case depth of 1 to 1.2 mm, respectively. 2. The thickness of the layer with over 58 Rc depends then on the subsequent heat treatment. The best treatment at which the very hard layer is thickest consists of quenching from 1000°C, a cold treatment at −70°C and tempering at 160° C (or 500° C).

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.