Abstract

The results of calculated and experimental studies of the influence of some parameters (the temperature and time of tritiation and aging, the cooling rate after tritiation) on the helium-3 concentration in metals are given. It has been experimentally found that the hydrogen concentration in [null]3 mm samples of 12Cr18Ni10Ti steel, which were saturated with hydrogen at 773 K and 50 MPa, makes up ~ 0.6 of the equilibrium hydrogen concentration immediately after cooling to room temperature and ~ 0.5 after 5000-hour aging.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.