Abstract
Amorphous oxide semiconductors have been widely studied for various applications, including thin-film transistors (TFTs) for display backplanes and semiconductor memories. However, the inherent instability, limited mobility, and complexity of multicomponent oxide semiconductors for achieving high aspect ratios and conformality of cation distribution remain challenging. Indium-zinc oxide (IZO), known for its high mobility, also faces obstacles in instability resulting from high carrier doping density and low ionization energy. To address these issues and attain a balance between mobility and stability, adopting a highly aligned structure such as a c-axis aligned crystalline IGZO could be advantageous. However, limited studies have reported enhanced electrical performance using crystalline IZO, likely attributed to the high thermal stability of the individual components (In2O3 and ZnO). Here, we first propose a c-axis aligned composite (CAAC) IZO with superior TFT properties, including a remarkable performance of field-effect mobility (μFE) of 55.8 cm2/(V s) and positive-bias-temperature-stress stability of +0.16 V (2 MV/cm, 60 °C, 1 h), as well as a low subthreshold swing of 0.18 V/decade and hysteresis as 0.01 V, which could be obtained through optimization of growth temperature and composition using thermal atomic layer deposition. These results surpass those of TFTs based on nanocrystalline/polycrystalline/amorphous-IZO. We conducted a thorough investigation of CAAC-IZO and revealed that the growth temperature and cation distribution profoundly influence the crystal structure and device properties. Finally, we observed excellent compositional conformality and 97% step coverage of IZO on a high-aspect-ratio (HAR) structure with an aspect ratio reaching 40:1, which is highly promising for future applications. Our results include a detailed investigation of the influence of the crystal structure of IZO on the film and TFT performance and suggest an approach for future applications.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.